Surface analysis of treated textiles
13
Apr 23

At a time when users want to consume less but better and when ecological and ethical concerns are on the rise, SERMA Science et surface has joined forces with ADEME for the AFTER project.

Its objective? To propose alternative solutions that support the relocation of production based on eco-efficient processes for functional textile finishing.

In the materials surface analysis laboratory, our teams carry out SEM, FTIR, XPS and wettability analyses that allow the chemical characterisation of fireproof, easy-care and water-repellent treatments of treated textiles.

The AFTER project allows SERMA Science et surface to provide a very advanced expertise in the understanding of the physico-chemical reaction mechanisms of the surface, all in compliance with REACH regulations.